  • SUPER DUPLEX S32760 / F55 / 1.4501

    Super Duplex S32760/ F55, Super Duplex Alloy UNS S32760 (F55 / 1.4501) ili ndi kukana kwabwino kwa Pitting ndi Crevice Corrosion m'madzi a m'nyanja pamatenthedwe okwera, operekedwa ndi PREN 40<(Pitting Resistance Eqv) . Kukaniza kwabwino kwa SCC (Stress Corrosion Cracking) m'malo a Sour ndi Chloride.

  • 17-7 Steel Strip, Coil, Foil, Waya, AMS 5528 (CONDA), AMS 5529 (COND C), ASTM A693, MIL-S25043

    ● Akasupe
    ● Ochapira
    ● Makapu
    ●Zigawo za opaleshoni
    ● Masamba
    ● Mavuvu
    ● Chisa cha uchi

  • Hastelloy B

    Hastelloy B ndi njira yolimba yolimbitsidwa, nickel-molybdenum alloy, yokhala ndi kukana kwambiri kuchepetsa malo monga mpweya wa hydrogen chloride, ndi sulfuric, acetic ndi phosphoric acid. Molybdenum ndiye gawo loyamba la alloying lomwe limapereka kukana kwa dzimbiri pakuchepetsa malo. Chitsulo cha nickel chitsulo ichi chingagwiritsidwe ntchito ngati chowotcherera chifukwa chimakana kupanga mapangidwe a carbide amtundu wa tirigu m'madera omwe amakhudzidwa ndi kutentha.

    Nickel alloy iyi imapereka kukana kwa hydrochloric acid pamlingo uliwonse komanso kutentha. Kuphatikiza apo, Hastelloy B2 ili ndi kukana kwabwino kwambiri pakubowola, kusweka kwa dzimbiri komanso kuukira kwa mipeni komanso kukhudzidwa ndi kutentha. Aloyi B amapereka kukana koyera sulfuric acid ndi angapo non-oxidizing zidulo.

  • Chitsulo chosapanga dzimbiri cha Austenite

    High Temperature Aloyi Chemical kapangidwe kake Kalasi C Si Mn SP Cr Ni Mo Cu N ena osaposa 904L 0.02 1 2 0.015 0.03 19~21 24~26 4~5 1~2 - 253Ma 0.05~253~21~0402.1. ~22 10~12 - - 0.14~0.2 Ce0.03~0.08 254SMo 0.02 0.8 1 0.01 0.03 19.5 ~20.5 17.5 ~18.5 6~ 18.5 6~ 2-05 N 0.03 1 2 0.03 0.04 20–22 23.5~ 25.5 6-7 ≤0.75 0.18-...
  • Wopangidwa, Wosalala, Mzere, Wozungulira, Wabwino, Wokutidwa ndi Waya Wopanda ASTM A167, AMS 5523

    Aloyi 310S ndi austenitic chromium nickel chitsulo chosapanga dzimbiri chomwe chimakhala ndi kukana kwa okosijeni wabwino komanso mphamvu pa kutentha kwakukulu muutumiki wopitilira mpaka 2000ºF (ngati kutsitsa mpweya wa sulfure kulibe). Imagwiritsidwanso ntchito pakanthawi kochepa kutentha mpaka 1900 ° F chifukwa imakana kuyambiranso ndipo imakhala ndi gawo locheperako lokulitsa. Izi zimachepetsa chizoloŵezi cha chitsulo kuti chiziwombera mu ntchito ya kutentha. Aloyi 310S ndi yofanana ndi aloyi 310 kupatula zomwe zili ndi mpweya wochepa kuti muchepetse mpweya wa carbide panthawi yowotcherera.

  • Mpweya Woumitsa Chitsulo Chosapanga dzimbiri

    High Temperature Aloyi Chemical zikuchokera Gulu C Si Mn SP Cr Ni Mo Cu Nb Al zina zosaposa 0Cr17Ni4Cu4Nb 0.07 1 1 0.035 0.03 15.5~17.5 3~5 - 3~5 0.15~15~0707070.45. 035 0.03 16 ~ 18 6.5~7.5 - ≤0.5 - 0.75~1.5 - 0Cr15Ni7Mo2Al 0.09 1 1 0.035 0.03 14~16 6.5~7.75 2~3 - 0.75b01N01 0.035 0.03 14-15.5 3.5-...
  • ZITHUNZI ZONSE ZOTHANDIZA 625

    Aloyi 625 ndi nonmagnetic , dzimbiri - ndi oxidation-resistant, nickel-based alloy. Kulimba kwake komanso kulimba kwake pakutentha kwa cryogenic mpaka 2000 ° F (1093 ° C) zimachokera makamaka kuchokera kuzitsulo zolimba zazitsulo zokanira, columbium ndi molybdenum, mu matrix a nickel-chromium. Aloyiyo imakhala ndi mphamvu zotopa kwambiri komanso kupsinjika-kudzimbiri kukana kukana ma chloride ayoni. Zina zomwe zimagwiritsidwa ntchito pa alloy 625 zimaphatikizapo zishango za kutentha, zida za ng'anjo, makina oyendetsa injini ya gasi, zoyatsira zoyatsira ndi zitsulo zopopera, zida zamafakitale, ndi ntchito zapadera zamadzi am'nyanja.

  • Chitsulo chosapanga dzimbiri 904L 1.4539

    Deta iyi imagwira ntchito pazitsulo zosapanga dzimbiri 904L / 1.4539 zotentha komanso zozizira zopindidwa ndi zingwe, zinthu zomalizidwa pang'ono, mipiringidzo, waya wopindidwa ndi mbiri komanso machubu opanda msoko ndi owotcherera pofuna kukakamiza.

  • Iconnel

    High Temperature Alloy Chemical kapangidwe kake Kalasi C Si Mn SP Cr Ni Fe Al Ti Cu Mo Nb ena osaposa Inconel600 0.15 0.5 0.5 1 0.015 0.03 14~17 maziko 6~10 - - ≤0.5 - - - Inconel601. 0 30 10 . 25 maziko 10~15 1~1.7 - ≤1 - - - Inconel625 0.1 0.5 0.5 0.015 0.015 20~23 maziko ≤5 ≤0.4 ≤0.4 - 8.1550 3.15 ≤3 0.2 0.35 0...
  • Hastelloy C-276 MATERIAL DATA MASHITA

    HASTELLOY C276, UNS N10276 imatengedwa kuti ndi aloyi ya nickel yosasunthika kwambiri yomwe ilipo. Aloyi C-276 alinso kwambiri kukana pitting, kupsinjika-kudzimbiri akulimbana, makamaka oyenera ntchito kutentha kwambiri, inorganic ndi organic zidulo kusakaniza zosafunika (monga formic acid ndi acetic acid), ndi madzi a m'nyanja zowononga chilengedwe.

  • Aloyi

    High Temperature Alloy Chemical kapangidwe kake Kalasi C Si Mn SP Cr Ni Fe Al Ti Cu Mo Nb ena osaposa Inconel600 0.15 0.5 0.5 1 0.015 0.03 14~17 maziko 6~10 - - ≤0.5 - - - Inconel601. 0 30 10 . 25 maziko 10~15 1~1.7 - ≤1 - - - Inconel625 0.1 0.5 0.5 0.015 0.015 20~23 maziko ≤5 ≤0.4 ≤0.4 - 8.1550 3.15 ≤3 0.2 0.35 0...
  • ALOY 600 MATRIAL DATA PETS

    INCONEL 600

    Inconel Alloy 600 Aloyi ya nickel-chromium yokhala ndi kukana kwa okosijeni wabwino pa kutentha kwambiri komanso kukana kusweka kwa chloride-ion stress-corrosion, dzimbiri ndi madzi oyera kwambiri, komanso dzimbiri la caustic. Amagwiritsidwa ntchito pazigawo za ng'anjo, popanga mankhwala ndi chakudya, mu engineering ya nyukiliya, komanso poyatsira ma electrode.

    UNS: N06600

    Chiwerengero cha anthu: 2.4816