Nitronic

Tsatanetsatane wa Zamalonda

Zolemba Zamalonda

High Temperature Alloy

◆Nitronic50 (S20910 / XM-19) ndi nitrogen-enhanced austenitic stainless steel, yomwe imagwiritsidwa ntchito makamaka mu petrochemical, nsalu, kukonza chakudya ndi mafakitale apanyanja.

◆Nitronic60 (S21800/Alloy218) ili ndi kukana kwa okosijeni kwapamwamba kwambiri komanso kutsika kwapang'onopang'ono, ndipo imagwiritsidwa ntchito makamaka polimbana ndi kuvala ndi kukanda mapini a aloyi ndi ma projekiti ena ofunikira.

Chemical zikuchokera

Gulu

C

Si

Mn

S

P

Cr

Ni

Fe

Mo

Ti

Cu

Nb

N

zina

palibe wamkulu kuposa

Nitronic50

0.06

1

4 ndi 6

0.03

0.04

20.5-23.5

11.5-13.5

maziko

1.5-3

0.1 ~ 0.3

0.2 ~ 0.4

-

Nitronic60

0.1

3.5-4.5

7; 9

0.03

0.04

16; 18

8; 9

maziko

-

-

-

-

0.08 ~ 0.18

-

Aloyi katundu osachepera

Gulu

boma

mphamvu yamakokedwe RmN/m㎡

Kuchuluka kwa Zokolola Rp0.2N/m㎡

Elongation As%

Brinell kuuma HB

Nitronic50

Yankho mankhwala

690

380

35

-

Nitronic60

Yankho mankhwala

600

320

35

-