SUPER DUPLEX S32760 / F55 / 1.4501
DESCRIPTION
1.Kupereka mphamvu zapamwamba kuposa zonse za austenitic ndi 22% Cr Duplex Stainless Steels UNS S32760 (F55) ndizoyenera kugwiritsa ntchito zosiyanasiyana m'mafakitale monga Mafuta & Gasi, CPI(Chemical Processing Industries), ndi malo a Marine.
UNS S32760 (F55 / 1.4501) yalembedwa mu NACE MR 01 75 chifukwa cha ntchito zowawasa komanso kulandira Chivomerezo cha ASME pakugwiritsa ntchito Pressure Vessel.
milingo yamphamvu ndi njira zosavuta zochiritsira zotentha ku Zinthu RH 950 ndi TH 1050. Mphamvu yapamwamba kwambiri ya Condition CH 900 imapereka zabwino zambiri pomwe ductility ndi magwiridwe antchito amaloledwa.Munyengo yake yochizira kutentha, aloyiyi imapereka zida zapadera pamatenthedwe mpaka 900 ° F (482 ° C).
Material Data Sheet
Aloyi | Super Duplex S32760 |
Zofunika No. | 1.4501 |
EN chizindikiro (chachidule) | X2CrNiMoCuWN25-7-4 |
UNS | UNS S32760 |
Chizindikiro cha ntchito cholembetsedwa | ASTM A182/F55 |
Chemical zikuchokera
C | Cr | Cu | Fe | Mo | Mn |
% | ≤ % | ≤ % | % | % | |
0.030 kukula | 24 <26 | 0.5 <1.0 | Chikumbutso | 3.0 <4.0 | 1.0 max |
N | Ni | P | S | Si | W |
% | % | % | % | ≤ % | % |
0.20 <0.30 | 6.0 <8.0 | 0.030 kukula | 0.010 max | 0.010 max | 0.50 <1.0 |
Katundu Wapadera
Young Modulus N/mm2 | Kachulukidwe kg/dm³: | Maginito Permeability |
199 x 10 | 7.81g/cm³ | 33 |
Kukaniza Kwabwino Kwambiri pamiyendo ndi kung'ambika / kukokoloka kwa dzimbiri
Zofotokozera
● EN 10088-3 1.4501
● ASTM A473 UNS S32760 Forgings
● ASTM A182 Kalasi F55 UNS S32760 Ma Flanges Opanga
● ASTM A240 UNS S32760 Mapepala ndi Plate
● ASTM A479 UNS S32760 Bar
● ASTM A276 UNS S32760 Condition A
● NACE MR 01-75
Zinthuzi zimabwera ndi certification ya 3.1.
3.2 certification zilipo ndi ndalama zowonjezera.
Mechanical Properties
0.2% Kupanikizika Kwaumboni (N/mm2 ) [ksi] osachepera 550 | 550 [79.8] |
Kulimba Kwambiri Kwambiri (N/mm2) [ksi] osachepera | 750 [108.8]] |
Elongation (%) osachepera | 25 |
Kulimba (HBN) | 270 max |
Kuchepetsa kwa Cross Section Area (%) osachepera | 45 |
Charpy V-notch Impact at ambient Temp (J) [ft.lb] | 80min [59min] |
Charpy V-notch Impact pa -46°C (J) [ft.lb] | 45av, 35mins [33av, 25.8min] |